项目 | 测试方法 | 指标 | ||
适用温度范围 | UL224 | -55~+150℃ | ||
纵向变化率 | ASTM D2671 | -10%~+10% | ||
拉伸强度 | ASTM D638 | ≥11.7MPa | ||
断裂伸长率 | ASTM D638 | ≥200% | ||
热空气老化 150℃/168h | 拉伸强度 | ASTM D638 | ≥10.4MPa | |
断裂伸长率 | ASTM D638 | ≥200% | ||
体积电阻率 | IEC 93 | ≥1.0×1012Ω.cm | ||
击穿电压 | UL224 | 2500V(60s)无击穿 | ||
热冲击 | 200℃/4h | 不滴流、无裂纹 | ||
冷冲击 | -65℃/4h | 不开裂 | ||
同心率 | ASTM D2671 | ≥70% | ||
耐油性(按照AS230536种液体检测) | 拉伸强度 | ASTM D638 | ≥10.4MPa | |
断裂伸长率 | ASTM D638 | ≥200% |
规格 (Size) | 扩张后 As Supplied(mm) | 完全收缩后 After Recovery(mm) | |
最小内径 (Min ID) | 最大内径 (Max ID) | 壁厚 (Wall Thickness) | |
Ф3.2 | 3.20 | 1.6 | 0.75±0.15 |
Ф4.8 | 4.80 | 2.4 | 0.82±0.15 |
Ф6.4 | 6.40 | 3.2 | 0.90±0.15 |
Ф9.5 | 9.50 | 4.75 | 1.02±0.20 |
Ф12.7 | 12.70 | 6.35 | 1.22±0.20 |
Ф19.1 | 19.05 | 9.55 | 1.45±0.28 |
Ф25.4 | 25.40 | 12.7 | 1.78±0.28 |
Ф38.1 | 38.10 | 19.0 | 2.41±0.41 |
Ф50.8 | 50.80 | 25.1 | 2.79±0.41 |